Titanium TP340

commercially pure (CP) Titanium

Available in four distinct grades (1, 2, 3, and 4), Titanium is classified by its corrosion resistance, ductility, and strength. CP Ti Gr. 1 has the highest corrosion resistance, formability, and lowest strength, whereas, CP Ti Gr. 4 offers the highest strength with moderate formability. The most desirable feature of our CP Ti is its ability to osseointegrate within the human body. Titanium also offers a higher strength-to-weight ratio and increased corrosion resistance compared to the stainless steel alloys, thus making it an attractive choice for medical applications.

 

Category: Tag:

Description

CP Grade 2 Titanium ,TP270C, TP340C, TP340H, TB340

Commercially pure titanium grades feature an excellent strength-to-density ratio and good corrosion resistance. This makes them suitable for the manufacture of components in weight-saving structures with reduced mass forces, and also for components requiring high corrosion resistance. In addition, thermal stresses in titanium structures are lower than in other metallic materials, due to the low thermal expansion of titanium. The materials are also widely used in the medical sector because of their outstanding biocompatibility.

 

TP340, JIS Pure Titanium Plate, 340 ~ 510 MPa

TP340 is pure titanium.Titanium is over 99%

All other elements are metals that account for less than 1%.
Whether it is hot rolling or cold rolling,

According to the manufacturing rolling, it is TP340H for hot and TP340C for cold.
TP340 is pure titanium for industrial use

It has good corrosion resistance, especially sea water resistance
, and is used in chemical, petroleum, and pulp paper manufacturing equipment.

Titanium features
light weight — specific gravity of 4.51, approximately 60% of iron (Fe)

Strong — no difference in strength from steel and
biocompatible — extremely low ion elution, very low metal ion allergy

Corrosion resistance to seawater
— optimal for use in seawater environments due to seawater resistance to seawater and processability — equal to steel in processability

Non-magnetic — Non magnetic
low thermal expansion — thermal expansion coefficient of 8.40, equivalent to glass or concrete

Compared to Al: 23.9 and ordinary steel 11.6,
you can see how low it is.

 

※ Thermal expansion coefficient When the temperature (heat) rises by 1 ℃, it refers to the
ratio between the expanded size and the size before expansion. There are linear expansion coefficient and volume (volume) expansion coefficient.
The coefficient of thermal expansion decreases as the amount of carbon increases and the amount of alloy increases.

Commodity Standard Symbol Finishing mathod mass
Plate JIS H4600 TP270C Cold Rolling 4.51
JIS H4600 TP340C Cold Rolling 4.51
JIS H4600 TP340H Hot Rolling 4.51
Bar JIS H4650 TB340C Cold Rolling 4.51
JIS H4650 TB340H Hot Rolling 4.51
JIS H4657 TF340 Forging 4.51
ASTM B348 Gr.5 6AL-4V 4.43
Pipe JIS H4635 TTP340W Welding 4.51

 

Chemical composition (%, max) MPa. %. min.
Symbol N C H Fe O Ti Tensile Yield Elong.
TB270 0.03 0.08 0.01 0.20 0.15 Remainder 270 ~ 410 165 27
TB340 0.03 0.08 0.01 0.25 0.20 Remainder 340 ~ 510 215 23
TB480 0.05 0.08 0.01 0.30 0.30 Remainder 480 ~ 620 345 18
TB550 0.05 0.08 0.01 0.5 0.40 Remainder 550 ~ 760 485 15

Our Sales & Supplier Network

Australia, Pakistan,  Malaysia, Singapore, Taiwan, China,Vietnam, Belgium, Japan, South Korea, Philippines, France, United Kingdom, Indonesia, Thailand, Hong Kong, China, Sweden, United States, Dubai, Finland, Brunei,Germany.

OUR MOTTO : ” WHY BUY A FULL BAR OR SHEET WHEN YOU JUST NEED A SMALL VOLUME?

Our specialty is to provide wide range of alloy steel with no minimum order.( no MOQ )