High Tensile Steel plate 4140QT

E Steel Sdn Bhd supply full range of Plastic mould Steel plate, Plastic Mould steel round bar , Carbon steel plate, Carbon steel round Bar,  Hot work steel , Cold Work Tool Steel, Special Steel ,Tool Steel ,Corrosion resistant Steel.

OUR MOTTO : ” Right Metal, Right Specification to Right Application “

Description

4140 High Tensile Steel, SCM440, 42CrMo4, 7225, EN19, SCM4

4140 is a 1% chromium – molybdenum medium hardenability general purpose high tensile steel – generally  supplied hardened and tempered in the tensile range of 850 – 1000 Mpa (condition T).

AISI 4140 is now available with improved machinability, which greatly increases feeds and/or speeds, while also extending tool life without adversley affecting mechanical properties.

Pre hardened and tempered 4140 can be further surface hardened by flame or induction hardening and by nitriding.

1.7225 is used extensively in most industry sectors for a wide range of applications such as:
Adapters, Arbors, Axle Shafts, Bolts, Crankshafts, Connection Rods, Chuck Bodies, Collets, Conveyor Pins & Rolls, Ejector Pins, Forks, Gears, Guide Rods, Hydraulic Shafts & Parts,Lathe Spindles, Logging Parts, Milling Spindles, Motor Shafts, Nuts, Pinch Bars, Pins Various, Pinions, Pump Shafts, Rams, Sockets, Spindles, Sprockets, Studs, Tool Holders, Torsion Bars, Worms etc..

DIN AISI JIS Chemical Composition
C Si Mn P S Co Cr Mo Ni V W Cu
42CrMo4 4140 SCM 440 0.37 to 0.44 0.15 to 0.35 0.65 to 1.10 < 0.04 < 0.03 0.75 to 1.20 0.15 to 1.25 < 0.25 < 0.35

 

4140 Steel Equivalent
Country USA German British Japan China Australia
Standard ASTM A29 DIN 17200 BS 970 JIS G4105 GB/T 3077 AS 1444
Grades 4140 1.7225/ 42crmo4 42CrMo4 SCM440 42CrMo 4140

 JIS SCM440 Steel Mechanical Properties

  • Tensile strength (kgf/mm²): ≧100
  • Yield strength (kgf/mm²): ≧85
  • Elongation (%): ≧12
  • Cross section reduction rate (%): ≧45
  • Impact value (J/cm2): ≧6
  • Hardness (Hb) : 285~352
4140 steel Heat Treatment 
  • Annealing: 830℃ Furnace Cooling
  • Normalization: 830~880℃ Air Cooling
  • Hardening: 830~880℃ Oil Cooling
  • Tempering: 530~630℃ Rapid Cooling